基于有限元分析的准晶磨料强化不锈钢表面钝化行为
陈永君1,2, 白妍1, 董闯2,3(), 解志文1, 燕峰1, 吴迪1
Passivation Behavior on the Surface of Stainless Steel Reinforced by Quasicrystal-Abrasive via Finite Element Simulation
CHEN Yongjun1,2, BAI Yan1, DONG Chuang2,3(), XIE Zhiwen1, YAN Feng1, WU Di1

图8. 不同磨料碾磨系数与抛光时间的关系

Fig.8. Smearing coefficient vs polishing time on stainless steel with three kinds of abrasives