羟基亚乙基二膦酸对20SiMn钢在含Cl-混凝土模拟孔隙液中的缓蚀行为
曹凤婷1,2, 魏洁1, 董俊华1(), 柯伟1, 王铁钢2, 范其香2
Corrosion Inhibition Behavior of 1-Hydroxyethylidene-1, 1-Diphosphonic Acid on 20SiMn Steel in Simulated Concrete Pore Solution Containing Cl-
CAO Fengting1,2, WEI Jie1, DONG Junhua1(), KE Wei1, WANG Tiegang2, FAN Qixiang2

图6. 20SiMn钢在1 mol/L NaCl饱和Ca(OH)2空白和添加1.441×10-4 mol/L HEDP溶液中膜层电阻(Rf)、电荷转移电阻(Rct)随浸泡时间的变化

Fig.6. Curves of Rf and Rct of 20SiMn steel with immersion time in 1 mol/L NaCl saturated Ca(OH)2 solution without and with 1.441×10-4 mol/L HEDP