带损伤环氧涂层钢筋在Cl-和碳化耦合作用下的腐蚀行为
魏洁1, 魏英华2, 李京2, 赵洪涛2, 吕晨曦2, 董俊华1(), 柯伟3, 何小燕3
Corrosion Behavior of Damaged Epoxy Coated Steel Bars Under the Coupling Effect of Chloride Ion and Carbonization
WEI Jie1, WEI Yinghua2, LI Jing2, ZHAO Hongtao2, LV Chenxi2, DONG Junhua1(), KE Wei3, HE Xiaoyan3

图8. 活化腐蚀体系S2、S4~S6中预制损伤涂层钢筋试样腐蚀坑中腐蚀产物的Raman光谱

Fig.8. Raman spectra of corrosion products in pits of steel bar specimen with prefabricated damaged coating in activated corrosion systems S2, S4~S6