带损伤环氧涂层钢筋在Cl-和碳化耦合作用下的腐蚀行为
魏洁1, 魏英华2, 李京2, 赵洪涛2, 吕晨曦2, 董俊华1(), 柯伟3, 何小燕3
Corrosion Behavior of Damaged Epoxy Coated Steel Bars Under the Coupling Effect of Chloride Ion and Carbonization
WEI Jie1, WEI Yinghua2, LI Jing2, ZHAO Hongtao2, LV Chenxi2, DONG Junhua1(), KE Wei3, HE Xiaoyan3

图7. 预制损伤涂层钢筋试样在S1~S6溶液中浸泡60 d后腐蚀坑纵截面轮廓图

Fig.7. Longitudinal section contour maps of pits in steel bar specimen with prefabricated damaged coating immersed in solutions S1~S6 (a~f) for 60 d