热浸镀锌高强汽车板界面组织对其拉伸断裂行为的影响
于家英1, 王华1, 郑伟森1, 何燕霖1(), 吴玉瑞2, 李麟1
Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors
YU Jiaying1, WANG Hua1, ZHENG Weisen1, HE Yanlin1(), WU Yurui2, LI Lin1

图11. 3种高强镀锌板与去锌板的力学性能

Fig.11. Ultimate tensile strength (UTS) (a), elongation (b) and product of strength and elongation (PSE) (c) of three high-strength coated and uncoated steels