Effect of the Interface Microstructure of Hot-Dip Galvanizing High-Strength Automobile Steel on Its Tensile Fracture Behaviors
|
|
图1. 原位分析时拉伸实验样品尺寸示意图 |
Fig.1. Schematic of tensile sample size for in situ analysis (unit: mm) |
![]() |