[an error occurred while processing this directive]
一种单晶高温合金的弹性性能的各向异性
刘金来(
), 叶荔华, 周亦胄, 李金国, 孙晓峰
Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy
LIU Jinlai(
), YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng
图6.
合金各向异性因子随温度的变化
Fig.6.
The variation of anisotropy ratio of the superalloy with temperature