一种单晶高温合金的弹性性能的各向异性
刘金来(), 叶荔华, 周亦胄, 李金国, 孙晓峰
Anisotropy of Elasticity of a Ni Base Single Crystal Superalloy
LIU Jinlai(), YE Lihua, ZHOU Yizhou, LI Jinguo, SUN Xiaofeng

图1. 剪切模量与取向关系的示意图

Fig.1. Schematics of dependence of shear modulus on orientation (l—the unit vector along primary orientation, m—the unit vector along secondary orientation, θ—the polar angle, ?—the azimuth angle, χ—the angle between m and line projected from l on horizontal plane then projected on the plane normal to l )
(a) definition of primary and secondary orientations in crystal coordinate system
(b) the relation between orientations and specimen geometry