U-Co与U-Fe基础体系非晶形成能力的比较 |
|||||||||||||||
| 黄火根, 张鹏国, 张培, 王勤国 | |||||||||||||||
|
Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems |
|||||||||||||||
| HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo | |||||||||||||||
| 表2 Fe与Co元素的物理化学性质对比 |
|||||||||||||||
| Table 2 Contrast of physical and chemical properties between Fe and Co |
|||||||||||||||
|
|||||||||||||||