U-Co与U-Fe基础体系非晶形成能力的比较
|
|
Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems
|
|
图4. 不同Cu辊线速率下U69.2Fe30.8合金样品的DSC曲线 |
Fig.4. DSC curves of U69.2Fe30.8 alloy samples prepared under different Cu-cooler linear rates |
![]() |