核电站DMWJ中材料拘束的影响与优化
|
|
杨杰, 王雷
|
Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants
|
|
YANG Jie, WANG Lei
|
|
表2 不同材料的Gurson-Tvergaard-Needleman (GTN)损伤参数[36]
|
Table 2 The Gurson-Tvergaard-Needleman (GTN) damage parameters of different materials[36]
|
|
| Material | q1 | q2 | q3 | εΝ | SN | fN | f0 | fC | fF |
|---|
| A508 | 1.5 | 1 | 2.25 | 0.3 | 0.1 | 0.002 | 0.00008 | 0.04 | 0.25 | | 316L | 1.5 | Variable | 2.25 | 0.3 | 0.1 | 0.002 | 0.000001 | 0.04 | 0.25 | | 52Mb | 1.5 | Variable | 2.25 | 0.3 | 0.1 | 0.002 | 0.000001 | 0.04 | 0.25 | | 52Mw | 1.5 | 1 | 2.25 | 0.3 | 0.1 | 0.002 | 0.00015 | 0.04 | 0.25 | | HAZ | 1.5 | 1 | 2.25 | 0.3 | 0.1 | 0.002 | 0.00015 | 0.04 | 0.25 | | FZ | 1.5 | 1 | 2.25 | 0.3 | 0.1 | 0.008 | 0.00080 | 0.01 | 0.15 | | NIZ | 1.5 | 1 | 2.25 | 0.3 | 0.1 | 0.002 | 0.00004 | 0.04 | 0.25 |
|
|
|