核电站DMWJ中材料拘束的影响与优化
|
|
杨杰, 王雷
|
Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants
|
|
YANG Jie, WANG Lei
|
|
表1 异种金属焊接接头4种材料的化学成分[35] (mass fraction / %)
|
Table 1 Chemical compositions of the four materials used for fabrication of the DMWJ[35]
|
|
| Material | C | S | P | Si | Mn | Ni | Cr | Mo | Cu | Al | Ti | Co | Fe | Nb |
|---|
| A508 | 0.200 | 0.001 | 0.005 | 0.20 | 1.36 | 0.96 | 0.17 | 0.47 | - | - | - | - | Bal. | - | | 316L | 0.025 | 0.001 | 0.005 | 0.52 | 1.73 | 11.69 | 17.89 | 2.43 | - | - | - | - | Bal. | - | | 52Mb | 0.020 | <0.001 | 0.003 | 0.14 | 0.25 | 60.39 | 28.91 | 0.01 | 0.01 | 0.67 | 0.56 | 0.01 | 9.03 | <0.01 | | 52Mw | 0.025 | 0.001 | 0.004 | 0.18 | 0.24 | 58.00 | 29.18 | 0.01 | 0.02 | 0.75 | 0.53 | 0.02 | 10.23 | <0.01 |
|
|
|