[an error occurred while processing this directive]
核电站DMWJ中材料拘束的影响与优化
杨杰(), 王雷
Effect and Optimal Design of the Material Constraint in the DMWJ of Nuclear Power Plants
YANG Jie(), WANG Lei

图8. 材料拘束失配系数Ms=0.5时的裂纹扩展路径

Fig.8. The crack growth path at Ms=0.5 (VVF—void volume fraction)
Color online