电磁振荡场作用下双辊铸轧制备2099Al-Li合金的偏析行为及组织性能
李师居1,2, 李洋1,2, 陈建强1, 李中豪1, 许光明1,2(), 李勇1, 王昭东1, 王国栋1
Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field
LI Shiju1,2, LI Yang1,2, CHEN Jianqiang1, LI Zhonghao1, XU Guangming1,2(), LI Yong1, WANG Zhaodong1, WANG Guodong1

图8. 带电粒子在电磁振荡场作用下的受力分析和枝晶碎断模型

Fig.8. Force analysis of charged particles under electromagnetic oscillation field and dendrite fragmentation model