[an error occurred while processing this directive]
电磁振荡场作用下双辊铸轧制备2099Al-Li合金的偏析行为及组织性能
李师居1,2, 李洋1,2, 陈建强1, 李中豪1, 许光明1,2(), 李勇1, 王昭东1, 王国栋1
Segregation Behavior, Microstructure and Properties of 2099Al-Li Alloy Produced by Twin-Roll Casting Underthe Action of Electromagnetic Oscillation Field
LI Shiju1,2, LI Yang1,2, CHEN Jianqiang1, LI Zhonghao1, XU Guangming1,2(), LI Yong1, WANG Zhaodong1, WANG Guodong1

图1. 电磁双辊铸轧工艺示意图和电磁双辊铸轧工艺实物图

Fig.1. Schematic of electromagnetic twin-roll casting (TRC) technique (a) and practicality diagram of electromagnetic TRC experimental device (b) (1—2099Al-Li alloy melt; 2—chute; 3—nozzle; 4—electromagnetic coil; 5—2099Al-Li alloy sheet; 6—roll; 7—cooling water; 8—pulsed electric field (PEF) wire; 9—pulse power supply)