[an error occurred while processing this directive]
选区激光熔化专用AlSiMg合金成分设计及力学性能
耿遥祥(), 樊世敏, 简江林, 徐澍, 张志杰, 鞠洪博, 喻利花, 许俊华
Mechanical Properties of AlSiMg Alloy Specifically Designed for Selective Laser Melting
GENG Yaoxiang(), FAN Shimin, JIAN Jianglin, XU Shu, ZHANG Zhijie, JU Hongbo, YU Lihua, XU Junhua

图6. SLM成形AlSiMg1.5样品纵剖面显微组织的SEM像

Fig.6. Longitudinal section SEM image of SLM-formed AlSiMg1.5 sample