[an error occurred while processing this directive]
二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图18. W50Cu50球磨粉末烧结前后的DSC曲线[109]

Fig.18. DSC curves of the 40 h milled W50Cu50 powder mixture before and after being annealed[109]