[an error occurred while processing this directive]
二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图16. 球磨30和40 h后在980 ℃烧结3 h制备的W50Cu50粉末的HRTEM像和相应的SAED花样[109]

Fig.16. HRTEM images of microstructures of theW50Cu50 sintered powder metallurgy materials prepared by milling for 30 h (a) and 40 h (c) and subsequent sintering at 980 ℃ for 3 h, and the corresponding SAED patterns of Figs.16a and c (b, d)[109] (Insets in Figs.16a and c show the EDX results of W50Cu50 sintered powders)