[an error occurred while processing this directive]
二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图15. W/Cu连接件界面显微结构的HRTEM观察结果[109]

Fig.15. HRTEM observation of the W/Cu interface of W/Cu joint prepared through the direct diffusion bonding[109]
Color online
(a) EDX line-scanning compositional profile
(b) HRTEM image at W/Cu interface
(c) filtered image of the region marked with blue rectangle in Fig.15b