二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图12. Mo/Ag层状复合材料截面的TEM像[101]

Fig.12. Cross-section TEM image for the Mo/Ag laminated sample annealed at 800 ℃ for 4 h (a) and the magnified image of the region marked with a white rectangular frame in Fig.12a (b)[101]