二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图11. 预退火的纯Mo和经过Ag离子注入的Mo的S参数比较、Mo/Ag层状金属基复合材料在不同温度退火的S参数和S/SB参数[101] (S为Doppler展宽谱的线性参数,SB为被归一化为无缺陷样品的S值)

Fig.11. Variable energy positron annihilation spectroscopy (VEPAS) results of various samples[101] (S is the line shape parameter of Doppler broadening data, SB is the parameter that is normalized to the defect-free S value)(a) S parameter vs positron implantation energy for the pre-annealed pure Mo and the Ag+ implanted Mo
(b) S parameter vs positron implantation energy for the pre-annealed pure Mo and the Mo/Ag laminated samples with a 100 nm thick Ag layer annealed at different temperatures