二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin

图8. W/Ag层状复合材料的界面结构[100]

Fig.8. Microscopic characterization for the interface of the W/Ag LMCs[100]