[an error occurred while processing this directive]
二元互不固溶金属合金化的研究进展
黄远(), 杜金龙, 王祖敏
Progress in Research on the Alloying of Binary Immiscible Metals
HUANG Yuan(), DU Jinlong, WANG Zumin
图7. Mo/Cu层状复合材料截面的EDX线扫描结果[100,102]
Fig.7. EDX line-scanning results of the cross-section of the Mo/Cu LMCs[100,102] Color online (a) drift corrected spectrum profile (b) EDX line-scanning profile along the red-line in Fig.7a