表2 ASPEX检测出的最大夹杂物尺寸和形貌
|
Table 2 Diameters and morphologies of the maximum inclusions in 24 specimens examined by ASPEX
|
|
| i | No.1 | No.2 | No.3 |
|---|
| xi / μm | Type | Figure | xi / μm | Type | Figure | xi / μm | Type | Figure | | 1 | 5.32 | Glo.-O |  | 4.95 | Glo.-O |  | 5.79 | TiN |  | | 2 | 5.85 | TiN |  | 5.26 | Al2O3 |  | 6.57 | TiN |  | | 3 | 6.65 | TiN |  | 5.90 | TiN |  | 6.97 | TiN |  | | 4 | 6.92 | Glo.-O |  | 6.08 | TiN |  | 7.02 | TiN |  | | 5 | 6.93 | TiN |  | 6.10 | Al2O3 |  | 7.14 | MnS |  | | 6 | 7.15 | Al2O3 |  | 6.99 | TiN |  | 7.79 | TiN |  | | 7 | 7.16 | Sul.-O |  | 7.89 | Sul.-O |  | 7.99 | Glo.-O |  | | 8 | 7.19 | Al2O3 |  | 7.90 | Al2O3 |  | 8.24 | TiN |  | | 9 | 7.69 | TiN |  | 7.93 | TiN |  | 9.01 | TiN |  | | 10 | 7.99 | TiN |  | 8.19 | Al2O3 |  | 9.37 | TiN |  | | 11 | 8.94 | TiN |  | 8.61 | TiN |  | 9.40 | TiN |  | | 12 | 9.48 | Glo.-O |  | 8.75 | TiN |  | 9.44 | TiN |  | | 13 | 10.77 | Glo.-O |  | 8.98 | MnS |  | 10.10 | TiN |  | | 14 | 10.96 | Glo.-O |  | 8.99 | Al2O3 |  | 10.63 | MnS |  | | 15 | 11.35 | TiN |  | 9.03 | Glo.-O |  | 11.47 | TiN |  | | 16 | 11.82 | TiN |  | 9.08 | Glo.-O |  | 11.53 | TiN |  | | 17 | 12.43 | Glo.-O |  | 9.13 | Sul.-O |  | 11.83 | TiN |  | | 18 | 12.85 | Glo.-O |  | 9.32 | TiN |  | 11.88 | TiN |  | | 19 | 14.21 | Sul.-O |  | 10.58 | Glo.-O |  | 12.37 | TiN |  | | 20 | 14.80 | TiN |  | 10.62 | Glo.-O |  | 12.49 | TiN |  | | 21 | 18.42 | MnS |  | 10.75 | TiN |  | 13.87 | Sul.-O |  | | 22 | 21.59 | Sul.-O |  | 11.53 | Glo.-O |  | 14.44 | Glo.-O |  | | 23 | 21.83 | TiN |  | 12.07 | TiN |  | 17.10 | TiN |  | | 24 | 29.10 | MnS |  | 15.68 | Glo.-O |  | 20.98 | Glo.-O |  |
|
|
|