图3. No.1~No.3钢中不同类型和尺寸的夹杂物典型分布

Fig.3. Distributions of the inclusions of different types and sizes in No.1 (a), No.2 (b) and No.3 (c) steels (X_ABS and Y_ABS—the abscissa and ordinate of inclusion measured on the sample surface, respectively)