[an error occurred while processing this directive]
超洁净轴承钢中夹杂物与滚动接触疲劳寿命的关系
孙飞龙1, 耿克2, 俞峰3, 罗海文1()
Relationship of Inclusions and Rolling Contact Fatigue Life for Ultra-Clean Bearing Steel
SUN Feilong1, GENG Ke2, YU Feng3, LUO Haiwen1()

图1. 统计极值(SEV)法估算的最大夹杂物特征尺寸结果

Fig.1. Estimating the characteristic sizes of maximum inclusions by the statistics of extreme values (SEV) method (x—inclusion size;S0—standard inspection area; G—Gumbel function; xv—characteristic size of the maximum inclusion (CSMI))
(a~c) linear fittings with 95% confidence intervals of No.1, No.2 and No.3 steels
(d) comparison of three SEV linear fittings