服役条件下镍基高温合金应力松弛微观机制
江河(),董建新,张麦仓,姚志浩,杨静
Stress Relaxation Mechanism for Typical Nickel-Based Superalloys Under Service Condition
JIANG He(),DONG Jianxin,ZHANG Maicang,YAO Zhihao,YANG Jing

图2. 不同合金的应力松弛曲线

Fig.2. Stress relaxation curves for different alloys (a) GH4169 and GH4169D (b) GH4738 and GH350