<111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响
胡斌,李树索,裴延玲,宫声凯(),徐惠彬
Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy
HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai(),XU Huibin

图6. [111]取向沿不同方向偏离的Schmid因子

Fig.6. Maximum Schmid factors of {111}<110> and {111}<112> slip systems for different orientations deviate from <111>(a) {111}<110> deviate along [1ˉ11]-[001] and [1ˉ11]-[011] boundary(b) {111}<112> deviate along [1ˉ11]-[001] and [1ˉ11]-[011] boundary