[an error occurred while processing this directive]
<111>取向小角偏离对一种镍基单晶高温合金蠕变性能的影响
胡斌,李树索,裴延玲,宫声凯(),徐惠彬
Influence of Small Misorientation from <111> on Creep Properties of a Ni-Based Single Crystal Superalloy
HU Bin,LI Shusuo,PEI Yanling,GONG Shengkai(),XU Huibin

图3. 试样A经标准热处理后沿(011ˉ)面纵剖示意图及组织形貌的SEM像