[an error occurred while processing this directive]
高温合金涡轮叶片定向凝固过程数值模拟研究进展
许庆彦(),杨聪,闫学伟,柳百成
Development of Numerical Simulation in Nickel-Based Superalloy Turbine Blade Directional Solidification
XU Qingyan(),YANG Cong,YAN Xuewei,LIU Baicheng

图3. 恒定拉速与变拉速条件下叶片温度场模拟结果[31]