高温合金盘锻件制备过程残余应力的演化规律及机制
毕中南1,2(),秦海龙1,2,董志国3,王相平3,王鸣3,刘永泉3,杜金辉1,2,张继1,2
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings
BI Zhongnan1,2(),QIN Hailong1,2,DONG Zhiguo3,WANG Xiangping3,WANG Ming3,LIU Yongquan3,DU Jinhui1,2,ZHANG Ji1,2

图13. GH4169合金不同温度下时效保温过程中收缩应变随时间的变化[38]

Fig.13. Alloy shrinkage strains at different ageing temperatures measured using dilatometry[38]