Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings
|
|
图18. 残余应力引起的盘件加工轴向变形及原理示意图 |
Fig.18. Residual stress caused axial deformation(a) after machining with free state and principle sketch (b) symmetry machining allowance (Δσtop and Δσbottom indicate residual stress difference near the upper surface and lower surface at wheel core, respectively) (c) asymmetry machining allowance |
![]() |