高温合金盘锻件制备过程残余应力的演化规律及机制
毕中南1,2(),秦海龙1,2,董志国3,王相平3,王鸣3,刘永泉3,杜金辉1,2,张继1,2
Residual Stress Evolution and Its Mechanism During the Manufacture of Superalloy Disk Forgings
BI Zhongnan1,2(),QIN Hailong1,2,DONG Zhiguo3,WANG Xiangping3,WANG Ming3,LIU Yongquan3,DU Jinhui1,2,ZHANG Ji1,2

图11. 时效过程中GH4169盘锻件中心位置残余应力的原位中子衍射测试结果[32]

Fig.11. Stress relaxation vs time in the center of the disk during the ageing treatment[32]