镍基铸造高温合金等轴晶凝固成形技术的研究和进展
张军1(),介子奇1,2,黄太文1,杨文超1,刘林1,傅恒志1
Research and Development of Equiaxed Grain Solidification and Forming Technology for Nickel-Based Cast Superalloys
ZHANG Jun1(),JIE Ziqi1,2,HUANG Taiwen1,YANG Wenchao1,LIU Lin1,FU Hengzhi1

图1. 浇注温度和微量元素对K4169高温合金流动性的影响[14]

Fig.1. Effects of pouring temperature and trace elements on fluidity of K4169 superalloy (Lf—fluidity length, Tp—pouring temperature)[14]