航空发动机用粉末高温合金及制备技术研究进展
|
|
Research Progress in Powder Metallurgy Superalloys and Manufacturing Technologies for Aero-Engine Application
|
|
图6. 不同粒径粉末颗粒轨迹图 |
Fig.6. Particle trajectory of powder with different particle diameters |
![]() |