航空发动机用粉末高温合金及制备技术研究进展
|
|
Research Progress in Powder Metallurgy Superalloys and Manufacturing Technologies for Aero-Engine Application
|
|
图2. FGH4103、FGH4104和FGH4097合金的显微组织 |
Fig.2. Microstructures of FGH4103 (a), FGH4104 (b) and FGH4097 (c) PM superalloys |
![]() |