| 表4 高性能变形高温合金涡轮盘材料化学成分对照表[46,47,48,49,50,51,52] |
| Table 4 Chemical compositions of high performance disc superalloys[46,47,48,49,50,51,52] (mass fraction / %) |
|
| Alloy | Co | Cr | W | Mo | Al | Ti | Nb | Fe | Ni | Ref. |
|---|
| GH4065 | 13.00 | 16.00 | 4.00 | 4.00 | 2.10 | 3.70 | 0.70 | 1.00 | Bal. | [46] | | GH4742 | 10.40 | 14.15 | - | 5.03 | 2.51 | 2.56 | 2.62 | 0.53 | Bal. | [47] | | GH4169G | - | 18.77 | - | 3.12 | 0.48 | 1.05 | 5.20 | Bal. | 52.65 | [48] | | FGH4096 | 12.96 | 16.01 | 4.01 | 4.02 | 2.21 | 3.75 | 0.75 | 0.20 | Bal. | [49] | | GH4282 | 10.00 | 20.00 | - | 8.50 | 1.50 | 2.10 | - | - | Bal. | [50] | | GH4141 | 11.00 | 19.00 | - | 10.00 | 1.50 | 3.10 | - | - | Bal. | [50] | | GH4738 | 13.50 | 19.00 | - | 4.30 | 1.50 | 3.00 | - | - | Bal. | [51] | | GH4586 | 11.68 | 18.09 | 3.05 | 8.11 | 1.65 | 3.31 | - | - | Bal. | [52] | | GH4720Li | 14.96 | 16.03 | 1.23 | 2.98 | 2.53 | 5.01 | - | - | Bal. | [52] | | GH4975 | 15.58 | 7.96 | 10.22 | 1.18 | 5.01 | 2.49 | 1.66 | 0.10 | Bal. | [52] | | GH4169 | 1.00 | 19.00 | - | 3.00 | 0.50 | 1.10 | 5.20 | Bal. | 53.00 | [52] |
|
|
|