国内变形高温合金研制进展
杜金辉1,吕旭东1,2(),董建新3,孙文儒4,毕中南1,2,赵光普1,邓群1,崔传勇4,马惠萍1,张北江1
Research Progress of Wrought Superalloys in China
DU Jinhui1,LV Xudong1,2(),DONG Jianxin3,SUN Wenru4,BI Zhongnan1,2,ZHAO Guangpu1,DENG Qun1,CUI Chuanyong4,MA Huiping1,ZHANG Beijiang1

图10. 涡轮盘超声C扫图

Fig.10. C-scan images of the turbine disk(a) C-scan of clutter distribution (b) time of flight (TOF) of clutter distribution (c) C-scan of bottom echo distribution