[an error occurred while processing this directive]
国内变形高温合金研制进展
杜金辉1,吕旭东1,2(),董建新3,孙文儒4,毕中南1,2,赵光普1,邓群1,崔传勇4,马惠萍1,张北江1
Research Progress of Wrought Superalloys in China
DU Jinhui1,LV Xudong1,2(),DONG Jianxin3,SUN Wenru4,BI Zhongnan1,2,ZHAO Guangpu1,DENG Qun1,CUI Chuanyong4,MA Huiping1,ZHANG Beijiang1

图9. GH4169合金热力耦合作用后γ"相变体选择行为与晶粒取向的关系[33]

Fig.9. Relationship between γ" variant selection and grain orientation after thermo-mechanical coupling experiment in GH4169 alloy[33](a) EBSD figure of grain orientation (b) [001] grain orientation (c) [111] grain orientation (d) [101] grain orientation