Research Progress of Wrought Superalloys in China
DU Jinhui
1
,LV Xudong
1,
2
(
),DONG Jianxin
3
,SUN Wenru
4
,BI Zhongnan
1,
2
,ZHAO Guangpu
1
,DENG Qun
1
,CUI Chuanyong
4
,MA Huiping
1
,ZHANG Beijiang
1
图5.
GH4720Li合金快锻开坯数值模拟
Fig.5.
Simulation of cogging of GH4720Li alloy