变形高温合金盘材及其制备技术研究进展
张北江(),黄烁,张文云,田强,陈石富
Recent Development of Nickel-Based Disc Alloys andCorresponding Cast-Wrought Processing Techniques
ZHANG Beijiang(),HUANG Shuo,ZHANG Wenyun,TIAN Qiang,CHEN Shifu

图14. 热模拟拉伸实验中GH4065合金铸态组织与双相细晶组织的断面收缩率对比

Fig.14. Hot working plasticity of alloy GH4065 characterized by percent area reduction of tension tests(a) as-cast structures after solutioning treatment (b) γ+γ' microduplex (c) schematic of original specimen