图6. GH4065合金直径300 mm棒材上观察到的通道偏析缺陷

Fig.6. A freckle identified on the billet of alloy GH4065 with diameter of 300 mm(a~c) macro-scale morphologies of the freckle under various conditions of incident light ((a, b) transverse, (c)longitudinal)(d~h) EPMA mappings of alloying elements distribution