镍基单晶高温合金的研发进展
|
|
Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys
|
|
图7. 利用X射线断层扫描(XCT)观察到的铸态和热等静压DD33单晶合金中的显微孔洞 |
Fig.7. Micro-porosities in as cast (a) and as hot isostatically pressed (HIPed) (b) DD33 superalloy |
![]() |