镍基单晶高温合金的研发进展
|
|
Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys
|
|
图1. 钴基合金与典型第一代镍基单晶合金持久性能对比 |
Fig.1. Creep rupture properties of Co-based alloys and the 1st generation Ni-based single crystal (SX) superalloys (T—temperature, K; t—time, h; P—Larson-Miller parameter) |
![]() |