我国典型金属间化合物基高温结构材料的研究进展与应用
宫声凯1(),尚勇1,张继2,郭喜平3,林均品4,赵希宏5
Application and Research of Typical Intermetallics-Based High Temperature Structural Materials in China
GONG Shengkai1(),SHANG Yong1,ZHANG Ji2,GUO Xiping3,LIN Junpin4,ZHAO Xihong5

图2. 铸造高铌TiAl合金的XRD谱及Larson-Miller蠕变曲线对比

Fig.2. XRD spectra of the cast TiAl-Nb alloys with different Al contents (a) and comparison of the Larson-Miller creep parameter of studied alloys (T—temperature, tf—time, P—Larson-Miller parameter) (b)