GH4169
合金圆盘时效过程残余应力的演化规律研究
秦海龙,张瑞尧,毕中南(
),杜洪标,张金辉
Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk
Hailong QIN,Ruiyao ZHANG,Zhongnan BI(
),Lee Tung Lik,Hongbiao DONG,Jinhui DU,Ji ZHANG
图11.
应力拟合分析误差随时效时间的变化
Fig.11.
Evolution of stress fitting error with increasing ageing time