GH4169合金圆盘时效过程残余应力的演化规律研究
|
|
Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk
|
|
图8. 保温时效过程中圆盘中心残余应力演化规律 |
Fig.8. Evolution of residual stress in the center of disk during isothermal ageing process on the basis of dynamic non-stress standard sample (a) and static non-stress standard sample (b) |
![]() |