GH4169合金圆盘时效过程残余应力的演化规律研究
|
|
Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk
|
|
图5. 固溶水淬后圆盘试样微观组织的OM和SEM像 |
Fig.5. OM (a) and SEM (b) images of the microstructures of disk after quenching |
![]() |