GH4169合金圆盘时效过程残余应力的演化规律研究
秦海龙,张瑞尧,毕中南(),杜洪标,张金辉
Study on the Evolution of Residual Stress During Ageing Treatment in a GH4169 Alloy Disk
Hailong QIN,Ruiyao ZHANG,Zhongnan BI(),Lee Tung Lik,Hongbiao DONG,Jinhui DU,Ji ZHANG

图3. 无应力s0试样示意图

Fig.3. Schematic of stress-free s0 sample