AZ31镁合金室温多道次压缩过程微观组织和织构演变的研究
邓丽萍1,崔凯旋2,汪炳叔2(),向红亮1,李强2
Microstructure and Texture Evolution of AZ31 Mg Alloy Processed by Multi-Pass Compressing Under Room Temperature
Liping DENG1,Kaixuan CUI2,Bingshu WANG2(),Hongliang XIANG1,Qiang LI2

图7. TD5.5%-RD5.0%和TD5.5%-RD5.0%-ND5.2%样品孪晶细化晶粒行为EBSD取向成像图和{0001}极图分析

Fig.7. Analyses of the twins refine grains with EBSD orientation mapping (a, c) and {0001} pole figures (b, d) of TD5.5%-RD5.0% (a, b) and TD5.5%-RD5.0%-ND5.2% (c, d) samples (TTD, TTD1 and TTD2—twins generated from M in 1st compression, TRD—twin generated from TTD in 2nd compression, TND1—twin generated from TRD in 3rd compression, TND2—twin generated from TTD in 3rd compression)Color online